KOMPOSISI KIMIA
incoloy 625 coiled tubing capillary tubing
C | Cr | Ni | Fe | Mn | Si | Mo | Co | P | S | Ti | Nb + Ta | Al |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤ 0.1 | 20 – 23 | ≥ 58 | ≤ 5 | ≤ 0,5 | ≤ 0,5 | 8 – 10 | ≤ 1* | ≤ 0,015 | ≤ 0,015 | ≤ 0.4 | 3.15 – 4.15 | ≤ 0.4 |
(massa%)
* Lamun ditangtukeun
ASTM B444, ASME SB444, AMS 5581
Pikeun ASTM B444, ASME SB444, AMS 5581
Kaayaan | Kakuatan regangan | Kakuatan ngahasilkeun | Elongation |
minimum, ksi | minimum, ksi | minimum,% | |
Kelas 1 | 120 | 60 | 30 |
Kelas 2 | 100 | 40 | 30 |
* Sipat kakuatan luhur bisa disadiakeun dina kaayaan hardened tiis.
incoloy 625 coiled tubing capillary tubing
70°F | 200°F | 400°F | 600°F | 800°F | 1000°F | ||
---|---|---|---|---|---|---|---|
Kapadetan | lbs / dina 3 | 0.305 | - | - | - | - | - |
Ékspansi termal | X10-6/°F | - | 7.1 | 7.3 | 7.4 | 7.6 | 7.7 |
Modulus elastis | 103 ksi | 30.1 | 29.6 | 28.7 | 27.8 | 26.9 | 25.7 |
Babandingan Poisson | - | 0.278 | 0.28 | 0.286 | 0.29 | 0.295 | - |
Konduktivitas termal | Btu-in/h·ft2·°F | 68 | 75 | 87 | 98 | 109 | 139 |
Panas spésifik | Btu/lb·°F | 0.098 | 0.102 | 0.109 | 0.115 | 0.122 | 0.118 |
Kakuatan ngahasilkeun | ksi | 70 | 68 | 63 | 60 | 59 | 34 |
Kakuatan regangan | ksi | 140 | 134 | 130 | 129 | 129 | 88 |
incoloy 625 coiled tubing capillary tubing
PROSESDESKRIPSISteel MakingElectric Arc Furnace dituturkeun ku Vacuum Oxygen Decarburization (VOD) atawa Argon Oxygen Decarburization (AOD).Bisa disadiakeun dina annealed, solusi annealed atawa kaayaan hardened tiis.Kaayaan annealed kakuatan anu langkung luhur biasana dianggo dina jasa dugi ka 1100 ° F, sedengkeun kaayaan annealed solusi dianggo dina aplikasi di luhur 1100 ° F.