Komposisi Kimia
Hastelloy C2000 8,0 * 1,25 mm coiled tubing
Komposisi kimia Hastelloy C-2000 dituduhkeun dina tabel di handap ieu:
unsur | Min% | Max % |
---|---|---|
Cr | 22.00 | 24.00 |
Mo | 15.00 | 17.00 |
Fe | – | 3.00 |
C | – | 0.01 |
Si | – | 0.08 |
Co | – | 2.00 |
Mn | – | 0.50 |
P | – | 0,025 |
S | – | 0.01 |
Cu | 1.30 | 1.90 |
Al | – | 0.50 |
Ni | bal |
Rincian alloy
Kapadetan Hastelloy C-2000, titik lebur, koefisien ékspansi, sareng modulus élastisitas dituduhkeun dina tabel di handap ieu:
Kapadetan | Titik lebur | Koéfisién ékspansi | Modulus of Rigidity | Modulus élastisitas |
---|---|---|---|---|
8,5 g/cm³ | 1399 °C | 12,4 μm/m °C (20 – 100 °C) | 79 kN/mm² | 206 kN/mm² |
0,307 lb/in³ | 2550 °F | 6,9 x 10-6dina/dina °F (70 – 212 °F) | 11458 ksi | 29878 ksi |
perlakuan panas bagian rengse
Hastelloy C2000 8,0 * 1,25 mm coiled tubing
Perlakuan panas has Hastelloy C-2000:
Kaayaan anu disayogikeun ku AWI | Tipe | Suhu | Waktos | Niiskeun |
---|---|---|---|---|
Annealed atanapi Spring Temper | Ngaleungitkeun Stress | 400 – 450 °C (750 – 840 °F) | 2 Hr | Hawa |
Hastelloy C2000 8,0 * 1,25 mm coiled tubing
Pasipatan
Sipat mékanis has Hastelloy C-2000:
Dianil | ||
---|---|---|
Kira-kira.kakuatan regangan | <1000 N/mm² | <145 ksi |
Kira-kira.suhu operasi gumantung kana beban ** jeung lingkungan | -200 nepi ka +400 °C | -330 nepi ka +750 °F |
Hastelloy C2000 8,0 * 1,25 mm coiled tubing
Spring Temper | ||
---|---|---|
Kira-kira.kakuatan regangan | 1300 – 1600 N/mm² | 189 – 232 ksi |
Kira-kira.suhu operasi gumantung kana beban ** jeung lingkungan | -200 nepi ka +400 °C | -330 nepi ka +750 °F |