Galunggung 20 Stainless Steel Coil Tubing Harga
Campuran 330 Komposisi
Campuran 20 Komposisi Kimia
Paduan 20 | Ni | C | Mo | Mn | Si | Fe | Cu | S | P | Cr |
32 – 38 | 0,02 max | 2 – 3 | 1 – 2 | 0,7 max | Bal | 3 – 4 | 0,005 max | 0,02 max | 19 – 21 |
alloy 20 Sipat mékanis
Kapadetan | Titik lebur | Kakuatan ngahasilkeun (0.2% Offset) | Kakuatan regangan | Elongation |
8,1 g/cm3 | 1443 °C (2430 °F) | Psi – 35000, MPa – 241 | Psi – 80000, MPa – 551 | 30% |
Alloy 20 titik lebur
Alloy 20 titik lebur | 1443 °C (2430 °F) |
Galunggung 20 Density | 8,1 g/cm3 |
Galunggung 20 Kakuatan Tensile | Psi – 80000, MPa – 551 |
Kakuatan ngahasilkeun (0.2% Offset) | Psi – 35000, MPa – 241 |
Elongation | 30% |
Galunggung 20 Sarimbag
STANDAR | UNS | WERKSTOFF NR. | AFNOR | EN | JIS | BS | GOST |
Paduan 20 | N08020 | 2.4660 | Z2NCUD31-20AZ | NiCr20CuMo | – | – | – |
Paduan 20 (UNS N08020)
Komposisi %
C Karbon | Mn Mangan | P Fosfor | S Walirang | Si Silikon | Ni Nikel | Cr Kromium | Mo Molybdenum | Cu Tambaga | Nb + Ta Niobium + Tantalum | Fe Beusi |
0,07 max | 2.00 max | 0,045 max | 0,035 max | 1.0 max | 32.00–38.00 | 19.00–21.00 | 2.0–3.0 | 3.0–4.0 | (8,0xC) - 1,0 maks | 35,0 max |
Toleransi dimensi
OD | OD Toleransi | Toleransi témbok |
.250” | ± .005" | ± 15% |
.375" | ± .005" | ± 15% |
.500” | ± .005" | ± 15% |
Sipat mékanis
Kakuatan ngahasilkeun: | 35 ksi mnt |
Kakuatan regangan: | 80 ksi mnt |
Elongation (min 2"): | 30% |
Poto Factoy
Pamariksaan
Pangiriman & Bungkusan
Laporan tés
Tulis pesen anjeun di dieu sareng kirimkeun ka kami